Quick Specs

Hempel Super Strength Glass Flake Epoxy 35840 belongs to glass flake coatings, an epoxy system. As a high-build coating used as its own primer, it is intended for highly corrosive environments. Hempel Super Strength Glass Flake Epoxy 35840 is a solvent-free, two-component, high-build, polyamine adduct-cured glass flake epoxy coating; the cured coating is hard, highly flexible, and has good abrasion resistance, seawater resistance and fresh water resistance. Parameters on this page: volume solids 100%, dry film thickness 500 µm, theoretical spreading rate 2 m²/L.

Parameter source: HEMPEL original technical data sheet (TDS) “Hempel Super Strength Glass Flake Epoxy 35840”; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.

This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.

Volume Solids100%
Dry Film Thickness500 µm
Theoretical Spreading Rate2 m²/L
VOC23 g/L (China)
Density / Specific Gravity1.3 kg/L
Number of ComponentsTwo-component
Flash Point87°C
Colour / AppearanceLight Grey 11150 **
Pot Life30 min

Browse Similar Models by CategoryThis model belongs to: Glass Flake, Epoxy

FAQ

How many components does Hempel Super Strength Glass Flake Epoxy have?
Hempel Super Strength Glass Flake Epoxy is a two-component product; mix according to the mixing ratio in the "Application Data" table on this page before use.
What dry film thickness is typically applied for Hempel Super Strength Glass Flake Epoxy?
The conventional dry film thickness of Hempel Super Strength Glass Flake Epoxy is 500 µm; the specific value is determined by the coating system and design requirements.
What is the theoretical spreading rate of Hempel Super Strength Glass Flake Epoxy?
The theoretical spreading rate of Hempel Super Strength Glass Flake Epoxy is 2 m²/L; actual consumption is adjusted according to substrate roughness, application loss and colour hiding power.
What is the volume solids of Hempel Super Strength Glass Flake Epoxy?
The volume solids of Hempel Super Strength Glass Flake Epoxy is 100%.
What is the VOC of Hempel Super Strength Glass Flake Epoxy?
The VOC of Hempel Super Strength Glass Flake Epoxy is 23 g/L (China).
What is the flash point of Hempel Super Strength Glass Flake Epoxy?
The flash point of Hempel Super Strength Glass Flake Epoxy is 87°C; storage, transport and application shall follow the product safety data sheet.
Which standards apply to Hempel Super Strength Glass Flake Epoxy?
As recorded in the technical data on this page: ISO 14025 (see the application instructions on this page); EN 15804 (see the application instructions on this page). Specific applicability is subject to the manufacturer's technical data sheet and the coating system.
Where can Hempel Super Strength Glass Flake Epoxy be purchased?
RichTech Industrial Technology (Shanghai) Co., Ltd. distributes industrial and marine coatings, representing brands including JOTUN, HEMPEL, International, PPG and KANSAI, and provides product selection, coating systems and quantity calculations. Company address: Changhui Building, 799 Yinxiang Road, Jiading District, Shanghai.

Product Characteristics

Description

Hempel Super Strength Glass Flake Epoxy 35840 is a solvent-free, two-component, high-build, polyamine adduct-cured glass flake epoxy coating; the cured coating is hard, highly flexible, and has good abrasion resistance, seawater resistance and fresh water resistance.

Recommended use

As a high-build coating used as its own primer, it is intended for highly corrosive environments. It can be used on pile foundations, offshore structures, splash zones and other immersed areas.

Service temperature

Certificates / approvals

- Third-party verified, product-specific Environmental Product Declaration (Type III EPD, ISO 14025, EN 15804)

Edition 6, System 7A, 7B. Edition 7, System 7A.

Product features

- Glass flake colour codes 1115G and 5063G meet the five-class requirements in ISO 24656 Annex D.

Product safetyFlash point 87°C

VOC content (after mixing the multi-component paint)

RegulationsValue
European Union23 g/L
USA (coatings)23 g/L
USA (regulatory)23 g/L
Canada23 g/L
China23 g/L
Hong Kong23 g/L
South Korea23 g/L

Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.

Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.

For professional use only.

Product Data

Product code35840
Product componentsBase 35849

Curing agent 95620_______________________________

Standard colour* / codeLight Grey 11150 **

Light Grey 11150

Volume solids100%
density1.3 kg/L
Recommended dry film thickness500 µm

_______________________________

Glass flake version / codeLight grey 1115G

Light grey 1115G

Volume solids100%
density1.3 kg/L
Recommended dry film thickness500 µm

Surface Preparation

Cleanliness

New construction

- Before final painting, all shop primer breakdown and contamination incurred during storage and erection must be thoroughly cleaned by mechanical/chemical means.

Maintenance and repair

Roughness

For further details, refer to the separate Hempel document Surface Preparation Guide.

Application

Mixing Ratio

Base 35849 : Curing agent 95620 (3 : 1 by volume)

Stir thoroughly before use. Thinning is not permitted.

Thinner

No thinning required

Cleaning solventHEMPEL's Tool Cleaner 99610

Pot Life

Product temperature20°C25°C30°C
Pot Life60 min36 min30 min

Recommended method

ToolsMaximum thinning volumeApplication parameters
Airless SprayNo thinning requiredNozzle pressure: 22 MPa Nozzle tip size: 0.53–0.69 mm
BrushNo thinning requiredNot applicable.

If brush or roller application is used, several coats may be required to achieve the specified dry film thickness. Spray parameters are indicative and may be adjusted to suit site conditions. Pressure figures apply to the material at 20 °C. (*For other application methods, consult the company representative.)

Film thickness

Specification rangeLowHighRecommended
Wet Film Thickness250 µm1001 µm501 µm
Theoretical Spreading Rate4 m²/L1 m²/L2 m²/L

Depending on the end use and service area, the product may be specified at film thicknesses other than those indicated. This will alter the spreading rate, drying and curing times and recoat interval. To achieve optimum performance, avoid excessive film thickness.

Application conditions

Relative humidity

Drying and recoat

Product compatibility

Previous coat: none, or according to Hempel's specification. Recommended product: HEMPEL Epoxy 15590. Subsequent coat: none, or according to Hempel's specification.

Drying Time

Surface temperature20°C
Hard Dry7 h
Through dry23 h
Fully cured7 days

Measured at 500 µm dry film thickness under standard conditions; see Hempel's explanatory notes.

Recoat

Hempel's specifications supersede all guidance shown in the recoat table.

Product name20°C
Atmospheric, severe
HEMPEL High-Strength Glass Flake Epoxy 35840Minimum8 h
Maximum30 days
HEMPEL's Polyurethane Mastic Topcoat 55610Minimum8 h
Maximum5 days
Immersion
HEMPEL High-Strength Glass Flake Epoxy 35840Minimum8 h
Maximum30 days

For products of the same generic chemical composition, recoat times are for reference only.

For further information, refer to Hempel's specifications.

Drying conditions

- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.

Recoat notes

Others

Storage

Shelf Life

Ambient temperature25°C
Binder36 months
Curing agent12 months

When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.

Storage conditions

- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.

Carbon footprint

GWP (Global Warming Potential)6.6 g CO₂e/m²

Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².

The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.

Calculated based on the standard colours defined in this PDS. Values may vary with colour.

NumberDocument descriptionLocation/Notes
3.PDSThis document

datasheet, which is also available for download at www.hempel.com.

Supplementary documents

For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:

- Application methods - General application guide. This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):

1.Technical declarationProvides one-off specific advice for the requirements of a specific project
2.SpecificationsIssued for specific projects only
4.Explanatory notes to the PDSAvailable for download at www.hempel.com, containing information related to product test parameters
5.Application guideIf available, provided at www.hempel.com
6.General technical guidelines (e.g. application and surface preparation)

If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.

Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.

Similar models from the same brand — glass flake coating, epoxy coating

View all HEMPEL models

Purchase & Documents

Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.

China production baseIndustrial & marine coatingsWorldwide delivery