Jotapipe FC 407 Epoxy Coating for Gas Pipelines 407 is an epoxy paint. Specially designed as a flow-enhancing lining coating for gas transmission pipelines in non-corrosive environments. It is specially designed as a lining coating for pipelines to reduce friction inside gas pipelines. Parameters on this page: volume solids 74 ± 2%, dry film thickness 60–100 µm, theoretical spreading rate 12–7 m²/L. Comparable products of the same brand: Balloxy HB Light Epoxy Ballast Tank Coating, Jota Armour Strong Abrasion-resistant Epoxy Non-slip Coating, Jotacote HF002 Universal Abrasion-resistant Epoxy HF.
Data source: JOTUN original Technical Data Sheet (TDS), "Jotapipe FC 407 Epoxy Coating for Gas Pipelines 407"; spreading rate and other values are converted from the TDS parameters, for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 74 ± 2% |
|---|---|
| Dry Film Thickness | 60–100 µm |
| Theoretical Spreading Rate | 12–7 m²/L |
| VOC | 248 g/L |
| Density / Specific Gravity | 1.38 kg/L |
| Number of Components | Two-component |
| Flash Point | 37 °C |
| Mixing Ratio | 2 parts : 1 part (by volume) |
| Shelf life | 12 months : 24 months |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Epoxy Coating for Gas Pipelines 407 (0J5)
This is a two-component polyamine-cured epoxy coating. It is a high-solids product. It is specially designed as a lining coating for pipelines to reduce friction inside gas pipelines.
It is used as a single-coat system only.
Specifically designed as a flow-efficiency internal lining for gas transmission pipelines in non-corrosive environments. Other
Complies with API RP 5L2 and meets ANSI/AWWA Standard C210-07 for water pipes.
Other certificates and approvals are available on request.
Red
| Property | Test / Standard | Description |
| Volume Solids | ISO 3233 | 74± 2 % |
| Flash Point | ISO 3679 Method 1 | 37 °C |
| Density | Theoretical Value | 1.38 kg/L |
| VOC — USA / Hong Kong | US EPA Method 24 (test value) (CARB (SCM) 2007, SCAQMD Rule 1113, Hong Kong) | 248 g/L |
| VOC — EU | IED (2010/75/EU) (theoretical value) | 234 g/L |
The data listed are based on factory batch production and may vary slightly with colour.
All data apply to the mixed paint only.
Typical recommended specification range
| Dry Film Thickness | 60–100 µm |
| Wet Film Thickness | 80–140 µm |
| Theoretical Spreading Rate | 12–7 m²/L |
The specific film thickness requirements should be determined by the customer/project specification.
To ensure lasting adhesion of the next coat, all surfaces must be clean, dry and free of contaminants.
Surface Preparation
| Substrate | Minimum | Recommended |
| Carbon Steel | Sa 2½ (ISO 8501-1); surface roughness 35–50 µm, rated “fine” per ISO 8503-2 | |
This product may be applied by the following methods
| Spray | Use two-component heated plural-component spray equipment or modified airless spray equipment (with a heater). |
|---|
| Epoxy 407 for Gas Pipelines, Component A | 2 parts |
| Epoxy 407 for Gas Pipelines, Component B | 1 part |
| Cleaner | JOTUN Thinner No. 17 |
|---|
When the thinner is used as a cleaning solvent, it must first comply with local regulatory requirements
In China, the cleaning solvent must comply with GB 38505-2020
| Nozzle tip size (inch/1000): | 21-26 |
| Nozzle pressure (minimum): | 180-240 bar/2600-3500 psi |
| Substrate Temperature | 10 °C | 23 °C | 40 °C |
| Touch Dry | 12 h | 7 h | 1.5 h |
| Handle dry | 32 h | 15.5 h | 5 h |
| Dry/cured to service | 9 days | 5 days | 3 days |
Drying and curing times are determined based on temperature and relative humidity below 85%, with dry film thickness within the average range.
| Touch Dry | The state at which light finger pressure leaves no mark or stickiness. |
|---|---|
| Handle dry | The minimum time after application before handling will not damage the film. |
Dry/cured to service: the minimum time before the coating can be permanently exposed to a specific environment/medium.
| Paint temperature | 23 °C |
| Pot Life | 60 min |
| Volume | Container Size | |
| (L) | ||
| Epoxy 407 for Gas Pipelines, Component A | 200 / 20 | |
| Epoxy 407 for Gas Pipelines, Component B | ||
Available in 1000 L IBC containers on special order. For details, contact your local Jotun company.
The packaging sizes above are typical reference sizes for factory batch production. Due to regional regulatory differences, packaging sizes and capacities may vary by region.
Store in accordance with national regulations. Keep in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
| Epoxy 407 for Gas Pipelines, Component A | 12 months |
| Epoxy 407 for Gas Pipelines, Component B | 24 months |
In some markets, the stated shelf life may be shortened to comply with local legal requirements. The above is the minimum shelf life; thereafter, testing is required to confirm quality remains acceptable.
For professional use only. Applicators and workers must be trained, experienced, capable and equipped to mix, stir and apply the coating correctly in accordance with JOTUN's technical documents. Applicators and workers must wear appropriate personal protective equipment when using this product. This guidance is provided based on current product knowledge. Any proposed modification to suit site conditions must be approved by the responsible JOTUN representative before use.
Read the safety warnings on the container packaging. Use in well-ventilated conditions. Avoid inhaling spray mist and avoid skin contact. In case of accidental splashes on skin, wash immediately with a suitable cleaner, soap and water. In case of eye contact, rinse thoroughly with water and seek medical attention immediately.
When used primarily as a primer or antifouling, products may show slight colour variation from batch to batch. Likewise, fading and chalking may occur when exposed to sunlight.
Gloss and colour retention of topcoats depend on the colour type, the surrounding environment such as temperature and UV intensity, and application quality.
Contact your local JOTUN office for further information.
The information in this datasheet is based entirely on knowledge gained in our laboratory and in practice. JOTUN products are regarded as semi-finished products, and their use is generally beyond our control. JOTUN therefore guarantees only the quality of the product itself. To comply with local regulations, the product may be adjusted, and we reserve the right to modify the datasheet without further notice.
Users should consult JOTUN for specific guidance on the suitability of the product for their requirements and applications.
In case of any discrepancy between language versions, the English (UK) version shall prevail.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.