← Back to JOTUN brand page
China-based coatings exporter — industrial & marine protective coatings from China's production bases

Jotapipe FC 400 Solvent-free Epoxy for Gas Lines 400

Quick Specs

Jotapipe FC 400 Solvent-free Epoxy for Gas Pipelines 400 is an epoxy coating. Specially designed as a flow-improving internal lining for gas transport pipelines in non-corrosive environments. It is specially designed as an internal lining for pipes, reducing friction within gas pipelines. Parameters on this page: volume solids 98 ± 2%, dry film thickness 100 µm, theoretical spreading rate 10 m²/L. Comparable products from the same brand: Balloxy HB Light Epoxy Ballast Tank Coating, Jota Armour Abrasion-resistant Epoxy Non-slip, Jotacote HF002 Universal Abrasion-resistant Epoxy HF.

Source: JOTUN original technical data sheet (TDS) "Jotapipe FC 400 Solvent-free Epoxy for Gas Pipelines 400"; spreading rate and other values are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.

This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.

Volume Solids98 ± 2%
Dry Film Thickness100 µm
Theoretical Spreading Rate10 m²/L
VOC101 g/L (China)
Density / Specific Gravity1.5 kg/L
Number of ComponentsTwo-component
Flash Point100 °C
Mixing Ratio2 parts : 1 part (by volume)
Shelf life12 months : 12 months

Browse Similar Models by CategoryThis model belongs to: Epoxy

FAQ

How many components does Jotapipe FC 400 have?
Jotapipe FC 400 is a two-component product. Mix according to the mixing ratio in the "Coating Data" table on this page before use.
What is the mixing ratio of Jotapipe FC 400?
The mixing ratio of Jotapipe FC 400 is 2 parts : 1 part (by volume).
What dry film thickness is normally applied for Jotapipe FC 400?
Jotapipe FC 400 is normally applied at 100 µm dry film thickness; the exact value is determined by the coating system and design requirements.
What is the theoretical spreading rate of Jotapipe FC 400?
The theoretical spreading rate of Jotapipe FC 400 is 10 m²/L; actual consumption varies with substrate roughness, application loss and colour hiding power.
What is the volume solids of Jotapipe FC 400?
The volume solids of Jotapipe FC 400 is 98 ± 2%.
What is the VOC of Jotapipe FC 400?
The VOC of Jotapipe FC 400 is 101 g/L (China).
What is the flash point of Jotapipe FC 400?
The flash point of Jotapipe FC 400 is 100 °C. Handle, store and apply in accordance with the product safety data sheet.
How long does Jotapipe FC 400 take to dry?
Drying time of Jotapipe FC 400 under standard conditions: touch dry 15 h; in practice affected by temperature, film thickness and ventilation.
Which standards apply to Jotapipe FC 400?
As recorded in the technical data on this page: ISO 3233 (see the application instructions on this page); ISO 3679 (see the application instructions on this page). Specific applicability is subject to the manufacturer's technical data sheet and the coating system.
Where can Jotapipe FC 400 be purchased?
RichTech Industrial Technology (Shanghai) Co., Ltd. distributes industrial and marine coatings, representing brands including JOTUN, HEMPEL, International, PPG and KANSAI, and provides product selection, coating systems and quantity calculations. Company address: Changhui Building, 799 Yinxiang Road, Jiading District, Shanghai.

Jotapipe FC 400

Product description

A two-component, solvent-free, polyamine-cured epoxy coating. It is specially designed as an internal lining for pipes, reducing friction within gas pipelines. It is applied as a single coat only.

Typical Use

Specifically designed as a flow-efficiency internal lining for gas transmission pipelines in non-corrosive environments. Other

Approvals and Certificates

Complies with API RP 5L2 and meets ANSI/AWWA Standard C210-07 for water pipes.

Other certificates and approvals are available on request.

Colour

Red

Product Data

PropertyTest / StandardDescription
Volume SolidsISO 323398± 2 %
Flash PointISO 3679 Method 1100 °C
DensityTheoretical Value1.5 kg/L
RegionRegulationsTest / StandardVOC Value
USCARB(SCM)2020 / SCAQMD rule 1113Calculation141 g/L
Hong KongAir Pollution Control (VOC) RegulationCalculation141 g/L
EUEuropean Paint Directive 2004/42/CECalculation141 g/L
ChinaGB 30981-2020 Limit of harmful substances of industrial protective coatingsGB/T 23985-2009 8.3101 g/L

The data listed are based on factory batch production and may vary slightly with colour.

Film Thickness per Coat

Typical recommended specification range

Dry Film Thickness100µm
Wet Film Thickness100µm
Theoretical Spreading Rate10m²/L

The specific film thickness requirements should be determined by the customer/project specification.

Surface Preparation

Surface Preparation Summary

Surface Preparation

SubstrateMinimumRecommended
Carbon SteelSa 2½ (ISO 8501-1); surface roughness 35–50 µm, rated “fine” per ISO 8503-2

Application

Application Methods

This product may be applied by the following methods

SprayUse two-component heated plural-component spray equipment or modified airless spray equipment (with a heater).

Mixing Ratio (by Volume)

Solvent-Free Epoxy 400 for Gas Pipelines, Component A2 parts
Solvent-Free Epoxy 400 for Gas Pipelines, Component B1 part

Thinner / Cleaning Solvent

CleanerJOTUN Thinner No. 17

When the thinner is used as a cleaning solvent, it must first comply with local regulatory requirements

In China, the cleaning solvent must comply with GB 38508-2020

Airless Spray Guidance

Nozzle tip size (inch/1000):18-24
Nozzle pressure:180-300 bar/2600-4300 psi

Drying and Curing Time

Substrate Temperature10 °C23 °C40 °C
Touch Dry15 h6 h1.5 h
Handle dry30 h12 h4 h
Dry/cured to service15 days7 days4 days

Drying and curing times are determined based on temperature and relative humidity below 85%, with dry film thickness within the average range.

Touch DryThe state at which light finger pressure leaves no mark or stickiness.
Handle dryThe minimum time after application before handling will not damage the film.

Dry/cured to service: the minimum time before the coating can be permanently exposed to a specific environment/medium.

Induction Time and Pot Life

Typical Packaging Sizes

VolumeContainer Size
(L)
Solvent-Free Epoxy 400 for Gas Pipelines, Component A10 / 20 / 20020 / 20 / 200
Solvent-Free Epoxy 400 for Gas Pipelines, Component B5 / 20 / 200

The packaging sizes above are typical reference sizes for factory batch production. Due to regional regulatory differences, packaging sizes and capacities may vary by region.

Storage

Store in accordance with national regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.

Shelf Life at 23 °C

Solvent-Free Epoxy 400 for Gas Pipelines, Component A12 months
Solvent-Free Epoxy 400 for Gas Pipelines, Component B12 months

In some markets, the stated shelf life may be shortened to comply with local legal requirements. The above is the minimum shelf life; thereafter, testing is required to confirm quality remains acceptable.

Precautions

For professional use only. Applicators and workers must be trained, experienced, capable and equipped to mix, stir and apply the coating correctly in accordance with JOTUN's technical documents. Applicators and workers must wear appropriate personal protective equipment when using this product. This guidance is provided based on current product knowledge. Any proposed modification to suit site conditions must be approved by the responsible JOTUN representative before use.

Health and Safety

Read the safety warnings on the container packaging. Use in well-ventilated conditions. Avoid inhaling spray mist and avoid skin contact. In case of accidental splashes on skin, wash immediately with a suitable cleaner, soap and water. In case of eye contact, rinse thoroughly with water and seek medical attention immediately.

Colour Variation

When used primarily as a primer or antifouling coating, products may show slight colour variation from batch to batch. Such products, and epoxy products used as topcoats, may chalk when exposed to sunlight.

Gloss and colour retention of topcoats depend on the colour type, the surrounding environment such as temperature and UV intensity, application quality and product type. Contact your local JOTUN office for further information.

Disclaimer

The information in this datasheet is based entirely on knowledge gained in our laboratory and in practice. JOTUN products are regarded as semi-finished products, and their use is generally beyond our control. JOTUN therefore guarantees only the quality of the product itself. To comply with local regulations, the product may be adjusted, and we reserve the right to modify the datasheet without further notice.

Users should consult JOTUN for specific guidance on the suitability of the product for their requirements and applications.

In case of any discrepancy between language versions, the English (UK) version shall prevail.

Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.

Similar models from the same brand — epoxy coating

View all JOTUN models

Purchase & Documents

Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.

China production baseIndustrial & marine coatingsWorldwide delivery