HEMPEL's Under-insulation Anti-corrosive 56990

Quick Specs

Hempel Heat-resistant Coating under Insulation 56990 belongs to Thermal Insulation Coatings. This product is specifically developed for the prevention of corrosion under insulation (CUI) and can be applied directly to steel substrates or zinc silicate primer. Complies with NACE SP0198 - 2017 Systems SS-5, CS-6 and CS-8. Parameters on this page: volume solids 76 ± 2%, dry film thickness 150 µm, theoretical spreading rate 5 m²/L. Comparable models from the same brand: Hempel Heat-resistant Coating under Insulation 275, Hempel Aerogel Thermal Insulation Coating 170, Hempel Aerogel Thermal Insulation Coating 175.

Parameter source: HEMPEL original technical data sheet (TDS) “Hempel Heat-resistant Coating under Insulation 56990”; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.

This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.

Volume Solids76 ± 2%
Dry Film Thickness150 µm
Theoretical Spreading Rate5 m²/L
VOC367 g/L (China)
Density / Specific Gravity—
Number of Components—
Flash Point25°C
ThinnerHEMPEL's Thinner 08080
Colour / AppearanceMetallic dark grey 10710 *

Browse Similar Models by CategoryThis model belongs to: Thermal Insulation

FAQ

What dry film thickness is typically applied for Hempel Heat-resistant Coating under Insulation?
The conventional dry film thickness of Hempel Heat-resistant Coating under Insulation is 150 µm; the specific value is determined by the coating system and design requirements.
What is the theoretical spreading rate of Hempel Heat-resistant Coating under Insulation?
The theoretical spreading rate of Hempel Heat-resistant Coating under Insulation is 5 m²/L; actual consumption is adjusted according to substrate roughness, application loss and colour hiding power.
What is the volume solids of Hempel Heat-resistant Coating under Insulation?
The volume solids of Hempel Heat-resistant Coating under Insulation is 76 ± 2%.
What is the VOC of Hempel Heat-resistant Coating under Insulation?
The VOC of Hempel Heat-resistant Coating under Insulation is 367 g/L (China).
What is the gloss of Hempel Heat-resistant Coating under Insulation?
The gloss of Hempel Heat-resistant Coating under Insulation is flat.
What thinner is used for Hempel Heat-resistant Coating under Insulation?
Recommended thinner for Hempel Heat-resistant Coating under Insulation: Hempel Thinner 08080.
What is the flash point of Hempel Heat-resistant Coating under Insulation?
The flash point of Hempel Heat-resistant Coating under Insulation is 25°C; storage, transport and application shall be carried out in accordance with the product safety data sheet.
Which standards are involved for Hempel Heat-resistant Coating under Insulation?
As recorded in the technical data on this page: measured in accordance with GB/T 23985-2009; new construction - abrasive blast cleaning to a minimum of Sa 2½ (ISO 8501-1) / SP 10 (SSPC) / NACE No.2. Specific applicability is subject to the manufacturer's technical data sheet and the coating system.
Where can Hempel Heat-resistant Coating under Insulation be purchased?
RichTech Industrial Technology (Shanghai) Co., Ltd. distributes industrial and marine coatings, representing brands including JOTUN, HEMPEL, International, PPG and KANSAI, and provides product selection, coating systems and quantity calculations. Company address: Changhui Building, 799 Yinxiang Road, Jiading District, Shanghai.

56990

Product Characteristics

Description

Hempel Heat-resistant Coating under Insulation 56990 is an MIO-tinted, fibre-reinforced inorganic copolymer coating that cures to form an inert multi-polymeric matrix (IMPM) and withstands temperatures and thermal shock/cycling up to 650°C [1200°F] in dry service or dry/wet service.

Complies with NACE SP0198 - 2017 Systems SS-5, CS-6 and CS-8. Approved under SaudiAramco APCS-11C.

Recommended use

Hempel Heat-resistant Coating under Insulation 56990 is recommended for long-term protection of hot pipes, equipment and other hot surfaces. This product is specifically developed for the prevention of corrosion under insulation (CUI) and can be applied directly to steel substrates or zinc silicate primer.

Service temperature

- Dry conditions or alternating dry/wet conditions: from -196°C [-321°F] to 650°C [1202°F].

Certificates / approvals

- Tested and evaluated according to NACE TM0174; standard test method for evaluating protective coatings for entry into service. Resistance to boiling tap water, Method B.

- Tested and evaluated according to the standard "Fire tests on building materials and structures"; flammability test method BS 476-5.

- Tested and evaluated according to the standard "Fire tests on building materials and structures"; determination of surface spread of flame of products, BS 476-7.

Product features

- Capable of withstanding temperatures and thermal shock/cycling up to 650°C [1200°F] in dry or dry/wet service.

Product safetyFlash point 25 °C

VOC content

RegulationsValue
European Union367 g/L
USA (coatings)366 g/L
USA (regulatory)366 g/L
Canada366 g/L
China367 g/L
Hong Kong366 g/L
South Korea367 g/L

For specific legislation, refer to the explanatory notes provided on the Hempel website hempel.com or the local Hempel website. Measured in accordance with GB/T 23985-2009. The volatile organic compound (VOC) value may vary depending on the colour shade; refer to Section 9 of the Safety Data Sheet. This product complies with the VOC requirements specified in national mandatory or national recommended standards; consult a company representative for details.

Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.

For professional use only.

Product Data

Product code56990

_______________________________

Standard colour / codeMetallic dark grey 10710 *
GlossFlat
Volume solids76 ± 2%

1.9 kg/L56990

Recommended dry film thickness150 µm

Aluminium colour / code

Pearl Light Grey / Pearl Grey 19360

Gloss

Refer to the Hempel Guide for Aluminium-containing Coatings.

Volume solids72 ± 2%

1.8 kg/L

Recommended dry film thickness150 µm

Surface Preparation

Cleanliness

New construction

- Abrasive blast clean to Sa 2½ (ISO 8501-1) / SP 10 (SSPC) / NACE No.2 minimum.

- Stainless steel, aluminium and other non-ferrous metals and alloys: use a non-metallic blast medium (e.g. corundum, garnet).

Maintenance and repair

- Clean thoroughly by hand or power tools to St 3 (ISO 8501-1) / SP 3 (SSPC). Avoid polishing.

Roughness

For further details, refer to the separate Hempel document Surface Preparation Guide.

Application

Mixing Ratio

Stir thoroughly before use.

ThinnerHEMPEL's Thinner 08080
Cleaning solventHEMPEL's Tool Cleaner 99610

HEMPEL's Thinner 08080

Recommended method

ToolsMaximum thinning volumeApplication parameters
Airless Spray5%Nozzle pressure: 17.5 MPa; nozzle size: 0.43–0.53 mm
Air Spray5%​-
Brush5%​-

If brush or roller application is used, several coats may be required to achieve the specified dry film thickness. Spray parameters are indicative and may be adjusted to suit site conditions. Pressure figures apply to the material at 20 °C. (*For other application methods, consult the company representative.)

Film thickness

Specification rangeLowHighRecommended
Dry Film Thickness100 µm225 µm150 µm
Wet Film Thickness132 µm297 µm198 µm
Theoretical Spreading Rate7.6 m²/L3.4 m²/L5 m²/L

56990

Application conditions

- If the temperature does not exceed 204 °C (400 °F) before or during use, refer to the Hempel technical guide or contact Hempel.

Relative humidity

Drying and recoat

Product compatibility

Drying Time

Surface temperature10°C20°C30°C40°C
Touch Dry90 min4530
Hard Dry4 h21½

Measured at 150 µm dry film thickness under standard conditions; see Hempel's explanatory notes.

Recoat

Hempel's specifications supersede all guidance shown in the recoat table.

Product name10°C20°C30°C40°C
Atmospheric, severe
Hempel Corrosion Under Insulation Coating 56990Minimum18 h6 h3 h2½ h
MaximumExtendable*

Extendable* Depending on the actual exposure conditions, the coated surface may be recoated after an extended time. Contact your local Hempel representative for advice.

For further information, refer to Hempel's specifications.

Drying conditions

- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.

Recoat notes

- When recoating Hempel Corrosion Under Insulation Coating 56990 itself, apply multiple thin coats to reduce the risk of coating blistering/pinholes.

Others

Storage

Shelf Life

Ambient temperature25°C
Product12 months

When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. The shelf life stated on the product label is determined according to local climatic conditions. For advice, consult Hempel.

Storage conditions

- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.

Carbon footprint

Dry Film Thickness1 µm
GWP (Global Warming Potential)7.1 g CO₂e/m²

Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².

The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.

56990

Supplementary documents

More information is available at the Knowledge Centre: https://www.hempel.com/knowledge-center. The following documents are in the “Technical Guidelines” section:

https://www.hempel.com/knowledge-center/technical-guidelines Hempel

NumberDocument descriptionLocation/Notes
3.PDSThis document

datasheet, which is also available for download at www.hempel.com.

This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):

1.Technical declarationProvides one-off specific advice for the requirements of a specific project
2.SpecificationsIssued for specific projects only
4.Explanatory notes to the PDSAvailable for download at www.hempel.com, containing information related to product test parameters
5.Application guideIf available, provided at www.hempel.com
6.General technical guidelines (e.g. application and surface preparation)

If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.

Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.

Similar models from the same brand — Thermal insulation

View all HEMPEL models

Purchase & Documents

Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.

China production baseIndustrial & marine coatingsWorldwide delivery