Hempel's Epoxy Paint 47200 is an epoxy coating. Used as a fast-drying primer or intermediate coat in an epoxy system, especially suitable for shop application requiring fast recoating. It has a short drying time, contains micaceous iron oxide and zinc phosphate, cures above -10 °C, and forms a tough abrasion-resistant film. Parameters on this page: volume solids 65 ± 2%; dry film thickness 100 µm; theoretical spreading rate 6.5 m²/L. Comparable products from the same brand: Hempel's Fibre-reinforced Strong Epoxy 47510, Hempel's Multipurpose Epoxy High-build 500 Winter-grade, Hempel's Multipurpose Epoxy High-build 500.
Source: HEMPEL original technical data sheet (TDS) 'Hempel's Epoxy Paint 47200'. Spreading rate and other values converted from the TDS; for reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 65 ± 2% |
|---|---|
| Dry Film Thickness | 100 µm |
| Theoretical Spreading Rate | 6.5 m²/L |
| VOC | 350 g/L (China) |
| Density / Specific Gravity | 1.5 kg/L |
| Number of Components | Two-component |
| Flash Point | 30°C |
| Thinner | HEMPEL's Thinner 08450 |
| Colour / Appearance | Grey 13610 |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Hempel's Epoxy Paint 47200 is a two-component epoxy paint cured with a polyamine adduct. It has a short drying time, contains micaceous iron oxide and zinc phosphate, cures above -10 °C, and forms a tough abrasion-resistant film.
Complies with EU Directive 2004/42/EC, the Paints Directive on limiting volatile organic compounds: subcategory j.
Used as a fast-drying primer or intermediate coat in an epoxy system, especially suitable for shop application requiring fast recoating. Can be specified for site application. Can also be specified where a longer recoat interval is required before applying polyurethane (normally used as a tie coat).
| Product safety | Flash point 30 °C |
|---|
| Regulations | Value |
| European Union | 350 g/L |
| USA (coatings) | 350 g/L |
| USA (regulatory) | 350 g/L |
| Canada | 350 g/L |
| China | 350 g/L |
| Hong Kong | 350 g/L |
| South Korea | 350 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. ªEU Directive 2004/42/CE. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 47200 |
|---|---|
| Product components | Base 47209 |
Hardener 97100
| Aluminium colour / code | Grey 13610 |
|---|
Refer to the Hempel Guide for Aluminium-containing Coatings.
| Volume solids | 65 ± 2% |
|---|---|
| density | 1.5 kg/L |
| Recommended dry film thickness | 100 µm |
For further details, refer to the separate Hempel document Surface Preparation Guide.
Base 47209 : Hardener 97100 (4:1 by volume)
Stir thoroughly before use. For multi-component products, use a container of suitable volume.
| Thinner | HEMPEL's Thinner 08450 |
|---|---|
| Cleaning solvent | HEMPEL's Tool Cleaner 99610 |
HEMPEL's Thinner 08450
| Product temperature | 20°C |
|---|---|
| Pot Life | 3 h |
| Tools | Maximum thinning volume | Application parameters |
| Airless Spray | 5% | Nozzle pressure: 15 MPa. Tip size: 0.38–0.53 mm |
| Air Spray | 15% | Tip size: 0.38 mm |
| Brush | 5% | Nozzle size: 0.53 mm |
If brush or roller application is used, several coats may be required to achieve the specified dry film thickness. Spray parameters are indicative and may be adjusted to suit site conditions. Pressure figures apply to the material at 20 °C. (*For other application methods, consult the company representative.)
| Specification range | Low | High | Recommended |
| Dry Film Thickness | 75 µm | 200 µm | 100 µm |
| Wet Film Thickness | 116 µm | 309 µm | 154 µm |
| Theoretical Spreading Rate | 8.6 m²/L | 3.2 m²/L | 6.5 m²/L |
Depending on the end use and service area, the product may be specified at film thicknesses other than those indicated. This will alter the spreading rate, drying and curing times and recoat interval. To achieve optimum performance, avoid excessive film thickness.
- To promote suitable application properties at low temperatures, allow the fully mixed base and curing agent to pre-react before application.
| Surface temperature | 20°C |
| Surface Dry | 20 min |
| Hard Dry | 120 min |
Measured at 100 µm dry film thickness under standard conditions; see Hempel's explanatory notes.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
| Ambient temperature | 25°C |
| Binder | 36 months |
| Curing agent | 24 months |
When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.
- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
| Dry Film Thickness | 1 µm | |
| GWP (Global Warming Potential) | 8.6 g CO₂e/m² |
Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².
The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.
Calculated based on the standard colours defined in this PDS. Values may vary with colour.
For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:
- Application methods - General application guide. This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.