China-based coatings exporter — industrial & marine protective coatings from China's production bases

HEMPEL's Water-borne Epoxy 184CN

Quick Specs

Hempel Water-borne Epoxy 184CN is a water-borne coating. Used as a general-purpose primer on steel structures (see Remarks). Hempel Water-borne Epoxy 184CN is a fast-drying water-borne two-component polyamine-cured epoxy primer. Parameters on this page: volume solids 56 ± 2%, dry film thickness 75 µm, theoretical spreading rate 7.5 m²/L. Comparable models from the same brand: Hempel Water-borne Epoxy 18500, Hempel Water-borne Epoxy 48140, Hempel Water-borne Epoxy 760.

Parameter source: HEMPEL original technical data sheet (TDS) “Hempel Water-borne Epoxy 184CN”; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.

This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.

Volume Solids56 ± 2%
Dry Film Thickness75 µm
Theoretical Spreading Rate7.5 m²/L
VOC51 g/L (China)
Density / Specific Gravity1.5 kg/L
Number of ComponentsTwo-component
Flash Point71°C
Colour / AppearanceLimestone Grey 12170 **
GlossFlat

Browse Similar Models by CategoryThis model belongs to: Water-borne, Epoxy

FAQ

How many components does HEMPEL water-borne epoxy have?
Hempel Water-borne Epoxy is a two-component product; use after mixing in the ratio given in the "Coating Data" table on this page.
What is the typical dry film thickness of HEMPEL water-borne epoxy?
Typical dry film thickness of HEMPEL water-borne epoxy is 75 µm; the exact value depends on the coating system and design requirements.
What is the theoretical spreading rate of HEMPEL water-borne epoxy?
The theoretical spreading rate of Hempel Water-borne Epoxy is 7.5 m²/L; actual consumption is adjusted for substrate roughness, application loss and colour hiding power.
What is the volume solids of HEMPEL water-borne epoxy?
The volume solids of Hempel Water-borne Epoxy are 56 ± 2%.
What is the VOC of HEMPEL water-borne epoxy?
The VOC of Hempel Water-borne Epoxy is 51 g/L (China).
What is the gloss of HEMPEL water-borne epoxy?
The gloss of Hempel Water-borne Epoxy is matt.
What is the flash point of HEMPEL water-borne epoxy?
The flash point of Hempel Water-borne Epoxy is 71 °C; storage, transport and application shall follow the product safety data sheet.
Which standards apply to HEMPEL water-borne epoxy?
As recorded in the technical data on this page: - the maximum permissible concentration of water-soluble salts tested in accordance with ISO 8502-9 is 50 mg/m² (expressed as NaCl); new construction: abrasive blast cleaning to a minimum of Sa 2½ (ISO 8501-1) / SP 10 (SSPC). Specific applicability is subject to the manufacturer's technical data sheet and the coating system.
Where can HEMPEL water-borne epoxy be purchased?
RichTech Industrial Technology (Shanghai) Co., Ltd. distributes industrial and marine coatings, representing brands including JOTUN, HEMPEL, International, PPG and KANSAI, and provides product selection, coating systems and quantity calculations. Company address: Changhui Building, 799 Yinxiang Road, Jiading District, Shanghai.

184CN

Product Characteristics

Description

Hempel Water-borne Epoxy 184CN is a fast-drying water-borne two-component polyamine-cured epoxy primer.

Cures to form a tough, anti-corrosive film.

Recommended use

Used as a general-purpose primer on steel structures (see Remarks).

Service temperature

Product safetyFlash point 71 °C

VOC content (after mixing the multi-component paint)

RegulationsValue
European Union51 g/L
USA (coatings)51 g/L
USA (regulatory)131 g/L
China51 g/L

Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.

Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.

For professional use only.

Product Data

Product code184CN
Product componentsBase 184C9

Curing agent 989CN

Standard colour* / codeLimestone Grey 12170 **

Light Grey 12170

GlossFlat
Volume solids56 ± 2%
density1.5 kg/L
Recommended dry film thickness75 µm

Surface Preparation

Cleanliness

- Before final painting, all shop primer breakdown and contamination incurred during storage and erection must be thoroughly cleaned by mechanical/chemical means.

- The maximum permitted water-soluble salt level tested in accordance with ISO 8502-9 is 50 mg/m² (as NaCl).

New construction

Maintenance and repair

184CN

Roughness

For further details, refer to the separate Hempel document Surface Preparation Guide.

Application

Mixing Ratio

Base 184C9 : Curing agent 989CN (3 : 4 by volume)

Stir thoroughly before use.

Thinner

Fresh water

Cleaning solventHEMPEL's Tool Cleaner 99610

Pot Life

Product temperature20°C
Pot Life2 h

Recommended method

ToolsMaximum thinning volumeApplication parameters
Airless Spray5%Nozzle pressure: 25 MPa Nozzle tip size: 0.38–0.48 mm
Brush5%Not applicable.
Air Spray10%Not applicable.

If brush or roller is used, multiple coats are required to obtain the specified dry film thickness. Do not thin the components separately — thinning after mixing is permitted. The pot life of water-borne two-component epoxy and polyurethane cannot be determined by the appearance change of the coating itself. In addition, unlike other coatings, the pot life shortens as the temperature decreases. Discard remaining paint beyond the pot life. Keep thinning to a minimum. Spray parameters are indicative and may be adjusted to site conditions. Pressure values apply to material at 20 °C. (*For other application methods, consult a company representative!).

Film thickness

Specification rangeLowHighRecommended
Dry Film Thickness50 µm100 µm75 µm
Wet Film Thickness89 µm179 µm134 µm
Theoretical Spreading Rate11 m²/L5.6 m²/L7.5 m²/L

To achieve optimum performance, avoid excessive film thickness. Depending on the end use and service area, the product may be specified at film thicknesses other than those indicated. This will alter the spreading rate, drying and curing times and recoat interval. The practical consumption factor may vary with application conditions, equipment and workmanship. Checking paint consumption against area improves film thickness control.

Application conditions

Relative humidity

Notes

- Before switching between solvent-borne and water-borne coatings, consult Hempel regarding pump cleaning.

- If brush or roller application is used, more coats are required to achieve the specified dry film thickness.

Drying and recoat

Product compatibility

184CN

Drying Time

Surface temperature20°C
Surface Dry30 min
Through dry3 h
Fully cured7 days

Measured at 75 µm dry film thickness under standard conditions; see Hempel's explanatory notes.

Recoat

Hempel's specifications supersede all guidance shown in the recoat table.

Product name10°C20°C30°C40°C
Atmospheric, mild
HEMPEL Water-Borne Polyurethane Topcoat 580Minimum10 h4 h2 h75 min
Maximum50 days20 days10 days6 days
HEMPEL's Water-borne Acrylic Mastic Enamel 58030Minimum10 h4 h2 h75 min
Maximum50 days20 days10 days6 days
HEMPEL's Water-borne Epoxy 184CNMinimum10 h4 h2 h75 min
MaximumExtendable*
Atmospheric, moderate
HEMPEL Water-Borne Polyurethane Topcoat 580Minimum20 h8 h4 h2½ h
Maximum25 days10 days5 days72 h
HEMPEL's Water-borne Acrylic Mastic Enamel 58030Minimum15 h6 h3 h110 min
Maximum17 days7 days3½ days51 h
HEMPEL's Water-borne Epoxy 184CNMinimum10 h4 h2 h75 min
MaximumExtendable*
Atmospheric, severe
HEMPEL Water-Borne Polyurethane Topcoat 580Minimum30 h12 h6 h3½ h
Maximum17 days7 days3½ days51 h
HEMPEL's Water-borne Acrylic Mastic Enamel 58030Minimum25 h10 h5 h3 h
Maximum17 days7 days3½ days51 h
HEMPEL's Water-borne Epoxy 184CNMinimum20 h8 h4 h2½ h
Maximum35 days14 days7 days4½ days

Extendable* Depending on the actual exposure conditions, the coated surface may be recoated after an extended time. Contact your local Hempel representative for advice.

For products of the same generic chemical composition, recoat times are for reference only.

For further information, refer to Hempel's specifications.

Drying conditions

- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.

Recoat notes

- Avoid exposing touch-up areas, full coats and intercoat intervals to high humidity during application.

Others

Storage

Shelf Life

Ambient temperature25°C
Binder12 months
Curing agent12 months

When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.

Storage conditions

184CN

Carbon footprint

Dry Film Thickness1 µm
GWP (Global Warming Potential)7.1 g CO₂e/m²

Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².

The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.

Calculated based on the standard colours defined in this PDS. Values may vary with colour.

Supplementary documents

For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:

NumberDocument descriptionLocation/Notes
3.PDSThis document

datasheet, which is also available for download at www.hempel.com.

This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):

1.Technical declarationProvides one-off specific advice for the requirements of a specific project
2.SpecificationsIssued for specific projects only
4.Explanatory notes to the PDSAvailable for download at www.hempel.com, containing information related to product test parameters
5.Application guideIf available, provided at www.hempel.com
6.General technical guidelines (e.g. application and surface preparation)

If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.

Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.

Similar models from the same brand — Water-borne, epoxy

View all HEMPEL models

Purchase & Documents

Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.

China production baseIndustrial & marine coatingsWorldwide delivery