HEMPEL Epoxy Primer 158CN is an epoxy coating used as a primer. Used as the primer in HEMPEL chlorinated rubber or acrylic, epoxy and polyurethane systems, for application to hot-dip galvanised, aluminium and stainless steel surfaces in moderately corrosive environments. It forms a flexible, well-adhering film with good abrasion resistance and impact resistance. Parameters on this page: volume solids 54 ± 2%, dry film thickness 40 µm, theoretical spreading rate 14 m²/L. Comparable models from the same brand: HEMPEL Epoxy Primer 1530C, HEMPEL Epoxy Shop Primer 15275, HEMPEL Epoxy Shop Primer 15280.
Parameter source: HEMPEL original technical data sheet (TDS) for HEMPEL Epoxy Primer 158CN; spreading rate and other values are converted from TDS parameters and provided for product selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 54 ± 2% |
|---|---|
| Dry Film Thickness | 40 µm |
| Theoretical Spreading Rate | 14 m²/L |
| VOC | 394 g/L (China) |
| Density / Specific Gravity | 1.4 kg/L |
| Number of Components | Two-component |
| Flash Point | 30°C |
| Thinner | HEMPEL Thinner 017CN |
| Colour / Appearance | Eggshell Grey 11320 |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
HEMPEL Epoxy 158CN is a two-component polyamide adduct-cured epoxy. It forms a flexible, well-adhering film with good abrasion resistance and impact resistance. The product contains zinc phosphate. It can cure at temperatures as low as 5 °C.
As a primer for use with HEMPEL chlorinated rubber or acrylic, epoxy and polyurethane coatings, applied over hot-dip galvanized, aluminium and stainless steel surfaces in medium corrosion environments. The product is also suitable for surfaces that cannot be abraded. See 'Surface Preparation'.
| Product safety | Flash point 30 °C |
|---|
| Regulations | Value |
| European Union | 394 g/L |
| USA (coatings) | 394 g/L |
| USA (regulatory) | 394 g/L |
| China | 394 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 158CN |
|---|---|
| Product components | Base 158C9 |
Curing agent 95HCN
| Standard colour / code | Eggshell Grey 11320 |
|---|
Light Grey 11320
| Volume solids | 54 ± 2% |
|---|---|
| density | 1.4 kg/L |
| Recommended dry film thickness | 40 µm |
For further details, refer to the separate Hempel document Surface Preparation Guide.
Base 158C9 : Curing agent 95HCN (3 : 1 by volume)
Stir thoroughly before use.
| Thinner | HEMPEL Thinner 017CN |
|---|---|
| Cleaning solvent | HEMPEL's Tool Cleaner 99610 |
| Product temperature | 20°C |
|---|---|
| Pot Life | 8 h |
| Tools | Application parameters |
|---|
Nozzle pressure: 17.5 MPa
Nozzle tip size: 0.43-0.48 mm. If brush or roller is used, multiple coats are required to achieve the specified dry film thickness. The spray parameters are indicative and may be adjusted according to site conditions. The pressure values apply to material at 20 °C. (*For other application methods, consult the company representative).
| Specification range | Low | High | Recommended |
| Wet Film Thickness | 55 µm | 92 µm | 74 µm |
| Theoretical Spreading Rate | 18 m²/L | 11 m²/L | 14 m²/L |
Depending on the end use and service area, the product may be specified at film thicknesses other than those indicated. This will alter the spreading rate, drying and curing times and recoat interval. To achieve optimum performance, avoid excessive film thickness.
| Surface temperature | 20°C |
| Fully cured | 7 days |
Dry film thickness 40 µm measured under standard conditions; see Hempel's explanatory notes for details. To determine the dry state, refer to the Application Specification COP FP1401-1 (drying test for high film thickness).
Hempel's specifications supersede all guidance shown in the recoat table.
| Product name | 10°C | 20°C | 30°C | 40°C | |
| Atmospheric, mild | |||||
|---|---|---|---|---|---|
| HEMPEL Acrylic High-Build Topcoat 460CN | Minimum | 75 min | 30 min | 15 min | 10 min |
| Maximum | 30 h | 12 h | 6 h | 3½ h | |
| Atmospheric, moderate | |||||
| HEMPEL Acrylic High-Build Topcoat 460CN | Minimum | 75 min | 30 min | 15 min | 10 min |
| Maximum | 30 h | 12 h | 6 h | 3½ h | |
| Atmospheric, severe | |||||
| HEMPEL Acrylic High-Build Topcoat 460CN | Minimum | 25 h | 10 h | 5 h | 3 h |
| Maximum | 30 h | 12 h | 6 h | 3½ h | |
For products of the same generic chemical composition, recoat times are for reference only.
For further information, refer to Hempel's specifications.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
| Ambient temperature | 25°C |
| Binder | 6 months |
| Curing agent | 24 months |
When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.
- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
| GWP (Global Warming Potential) | 9.6 g CO₂e/m² |
|---|
Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².
The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.
Calculated based on the standard colours defined in this PDS. Values may vary with colour.
For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:
- Application methods - General application guide. This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.