5917K SEA GRANDPRIX CF-10 Tin-free Copper-free Self-polishing Antifouling Paint belongs to antifouling paints. Good antifouling performance derives from a highly active polymer, which ensures greater efficacy and release of the biocide. Parameters on this page: volume solids 45 ± 2% (by volume) (ISO: 3233), dry film thickness 75–160 µm, theoretical spreading rate 0.167–0.356 L/m². Comparable models from the same brand: 4010B SEATENDER 7 Tin-free Self-polishing Antifouling Paint, 5843A SEAFLO NEO SL Tin-free Self-polishing Antifouling Paint, 5843H SEAFLO NEO SL Z Tin-free Self-polishing Antifouling Paint.
Parameter source: CMP original technical data sheet (TDS) “5917K SEA GRANDPRIX CF-10 Tin-free Copper-free Self-polishing Antifouling Paint”; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 45 ± 2% (by volume) (ISO 3233) |
|---|---|
| Dry Film Thickness | 75–160 µm |
| Theoretical Spreading Rate | 0.167-0.356 L/m2 |
| VOC | 545 g/L (Method 24) |
| Density / Specific Gravity | 1.38 g/ml (ISO: 2811) |
| Number of Components | One-component |
| Flash Point | 25.0°C |
| Thinner | CR/ACRI THINNER A |
| Colour / Appearance | Red, light red, purple |
SEA GRANDPRIX CF-10 is a tin-free, copper-free self-polishing antifouling paint based on a special resin. Designed for deep-sea vessels.
Good antifouling performance derives from the highly active polymer, which ensures high efficacy and release of the biocide.
Provides long-term antifouling protection through a controlled hydrolysis maintaining surface activity.
The product complies with the IMO Antifouling System Convention (AFS/CONF/26).
| Type | Tin-free, copper-free self-polishing antifouling |
|---|---|
| Use | Antifouling paint for the underwater hull of ocean-going vessels. (Mainly for newbuildings or repair vessels with thorough abrasive blasting) |
| Colour | Red, light red, purple |
|---|---|
| Flash Point | 25.0°C |
| Density | 1.38 g/ml (ISO: 2811) |
| Volume Solids | 45 ± 2% (by volume) (ISO 3233) |
| Volatile organic compound content | 545 g/L (Method 24) |
| Theoretical spreading rate | 0.167-0.356 L/m2 |
| Thickness | WFT 167–356 µm, DFT 75–160 µm |
(dry film 125 µm)
| Temperature | -5 °C | 0 °C | 5 °C | 10 °C | 20 °C | 30 °C | |
| Drying Time | Surface Dry | 6 h | 4 h | 3 h | 2 h | 1 h | 30 min |
| Hard Dry | 22 h | 16 h | 12 h | 8 h | 5 h | 4 h | |
| Recoat interval | At least | 22 h | 16 h | 12 h | 8 h | 5 h | 4 h |
| At most | / | / | / | ||||
| Dry-to-launch time | Fastest | 48 h | 36 h | 24 h | 18 h | 12 h | 10 h |
| Application method | Airless spray, brush, roller |
|---|---|
| Weather: temperature | Minimum -5 °C |
| Humidity | Maximum 85% RH |
| Airless spray: viscosity | 1.5 - 2.5 Pa.s |
| Nozzle | (Graco)621-723 |
| Paint output pressure | 11.7-14.7MPa |
| Spray gun speed | 60–80 cm/s |
| Thinner | CR/ACRI THINNER A |
| Thinning | 0–7% by volume for airless spray |
| 0–5% by volume | For brush and roller application: SILVAX SQ-K, RAVAX AC-HB, BANNOH 500 N, BANNOH 500 R, BANNOH previous coat coatings |
500 S and other models
| Subsequent coat | SEA GRANDPRIX CF Series, SEA GRANDPRIX CF SUPER |
|---|---|
| Packaging | One-component |
Note: 1. Expected antifouling performance during berthing: consider the ship's operating conditions and the berthing environment, such as marine growth activity, pollution level and water temperature at the berth. For details, consult the local CMP office.
2. Below 10 °C, additional thinner may be required to obtain a suitable application viscosity.
3 However, addition of excessive thinner will reduce sag resistance and film performance.
4. Density, solids content and VOC content are measured without added thinner.
Values vary with colour or production process.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.