Marine Antifouling Paint XH5905-4 is an antifouling paint. A ship bottom antifouling paint based on chlorinated rubber resin, with cuprous oxide, bioactive agents etc. Parameters on this page: volume solids 55 ± 2%, dry film thickness 80/100/120 µm, theoretical spreading rate 4.6 m²/L.
Parameter source: T&H manufacturer's Technical Data Sheet (TDS) "Marine Antifouling XH5905-4"; spreading rate and other values are converted from the TDS parameters and provided for product selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 55 ± 2% |
|---|---|
| Dry Film Thickness | 80/100/120 µm |
| Theoretical Spreading Rate | 4.6 m2/L |
| VOC | 370g/L |
| Density / Specific Gravity | 1.62 kg/L |
| Number of Components | One-component |
| Flash Point | 25°C |
| Thinner | 0-5% |
| Colour / Appearance | Red-brown or dark green |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Curing agent: none
A ship bottom antifouling paint based on chlorinated rubber resin, with cuprous oxide, bioactive agents etc.
| Colour | Red-brown or dark green |
|---|---|
| Gloss | Flat |
| density | 1.62 kg/L |
| Volume Solids | 55±2% |
| Volatile Organic Compounds | 370g/L |
| Flash Point | 25°C |
| Typical dry film thickness | 100µm |
|---|---|
| Recommended dry film thickness | 150–200 µm, depending on system requirements |
| Thinner quantity (by volume) | Airless spray 5–10% | Air spray 10–20% | Roller or brush 0–5% |
| Recommended nozzle size | 0.43~0.64mm | 1.5~2.5mm | / |
| Recommended spray pressure | 15~20MPa | 0.3~0.6MPa | / |
| Application suitability | Recommended | For small-area repair only | |
| Dry film thickness (µm) | 80 | 100 | 120 |
| Wet film thickness (µm) | 145 | 180 | 220 |
| Theoretical spreading rate (m²/L) | 6.9 | 5.5 | 4.6 |
| Temperature | Surface Dry | Hard Dry | Pot Life | Recoat interval | |
| Minimum | Maximum* | ||||
| 5°C | 4h | 16h | / | 24h | / |
| 15°C | 2h | 8h | / | 8h | / |
| 25°C | 1h | 4h | / | 6h | / |
| 40°C | 1h | 4h | / | 6h | / |
*The maximum recoat interval depends on the exposure environment and the end use of the coating.
The intermediate coat must be dry, with the surface free of oil, dust and other debris. Before coating, all surfaces shall be assessed and treated in accordance with ISO 8504:2000.
1. During application, ensure adequate ventilation and exhaust, keep away from sources of ignition, and wear protective equipment such as masks and gloves; maintain adequate ventilation also during curing. 2. Adjust the amount of thinner according to temperature changes, mix thoroughly and uniformly, and filter through a 120-mesh copper wire sieve before use. Unused paint must be sealed when not used for a long time, otherwise skinning is likely. If skinning occurs, the skin can be filtered out of the paint before use. 3. The film thickness of this product can be adjusted according to the purpose and location of use. This will change the spreading rate, drying time and overcoating interval. The normal range for one-coat dry film thickness is about 100 µm. Apply in 2 passes, with a total antifouling film thickness of 150–200 µm. 4. Because this product is a thermoplastic product, the film will dent under prolonged mechanical action at temperatures above about 40 °C. Once the temperature drops, the mechanical strength of the film recovers. 5. During application and curing, the substrate temperature must be above 5 °C and at least 3 °C above the dew point, and the relative humidity must not exceed 85%. Temperature and relative humidity shall be measured on the substrate close to the work point. 6. Cutting structures coated with this coating produces fumes and dust; appropriate protection shall be used. 7. When work is interrupted, do not leave paint in the hose, spray gun or spray equipment. Flush all equipment thoroughly with thinner. 8. All equipment shall be cleaned with thinner immediately after use. Flushing the spray equipment periodically during daily work is good practice. The cleaning frequency depends on spray volume, temperature, spraying time and interruptions. 9. Leftover paint and empty cans shall be disposed of according to local regulations.
20kg/12.3L
Keep sealed in a ventilated, cool, dry place away from sources of ignition. Minimum 12 months.
1. For the coating and its recommended thinners, see the safety sheets and the safety data of the relevant materials. This is a solvent-borne coating; avoid inhaling spray mist and solvent vapours, and avoid exposing skin and eyes and contact with uncured paint as far as possible. 2. All work related to the application and use of this product must comply with the relevant national health, safety and environmental standards and regulations. 3. If welding or flame cutting is required on metal coated with this product, dust and fumes will be generated; use appropriate personal protective equipment and adequate local ventilation. 4. If in doubt about the suitability of this product, consult the company.
The information provided in this product data sheet is based on laboratory test results that we consider accurate, and is provided for application guidance only. All recommendations and advice given by T&H on the use of T&H products, whether in technical documents, special consultation or otherwise, are based on information we consider most reliable. Our products and the information provided are intended for users with the necessary knowledge and industrial experience, and it is for these end users to determine whether the products are suitable for their use. T&H cannot control the quality and condition of the substrate, nor the various factors affecting the use of the product. Therefore, T&H accepts no liability for any loss, injury or damage arising from the use of our products or from reliance on this product data sheet (unless otherwise agreed in writing). Data in this product data sheet may be revised as necessary based on practical experience and continued product development.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.