Quick Specs

NOA PC antifouling belongs to antifouling coatings. The 1st Buff colour features Self Indicating (SI) technology, which lets a painter visually judge whether the correct film thickness (wet/dry) has been achieved during application. Parameters on this page: volume solids 65 ± 2%, dry film thickness 125-300 µm, theoretical spreading rate 5.20 m²/L.

Data source: nippon-marin original Technical Data Sheet (TDS), "NOA PC Antifouling Paint"; spreading rate and other values are converted from the TDS parameters, for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.

This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.

Volume Solids65 ± 2%
Dry Film Thickness125-300 µm
Theoretical Spreading Rate5.20 m²/L (125 µm)
VOC321 g / L as supplied
Density / Specific Gravity—
Number of ComponentsTwo-component
ThinnerNIPPON MARINE THINNER 600 / NIPPON …
Mixing RatioBASE 3.57 / HARDENER 1
Colour / Appearance1st coat : Buff

Browse Similar Models by CategoryThis model belongs to: Antifouling

A two-pack pure epoxy designed for petroleum and chemical product tanks.It offers superior resistance to petroleum products, solvents, water and chemical attack.

1st Buff color is characterized by Self Indicating (SI) technology, which enables a painter to visually judge if the correct film thickness (wet / dry) has been achieved during the application process and

after the completion of painting.Two coat system with SI paint (1st coat) plus non-SI paint (2nd coat) is recommended.

Suitable Use

Product Carriers, Tanks for petroleum products

TypePure epoxy (Two-pack)
Color1st coat : Buff
2nd coatGray (Non-SI)
GlossSemi-gloss
Volume Solids65 ± 2% (ISO3233:1998)
Dry Film Thickness125 ~ 300 µm
Approx. Wet Film Thickness192 ~ 462 µm
Theoretical Coverage5.20 m² / L (125 µm)
Drying TimeSurface Dry31/2 hours(5°C)11/2 hours(20°C)40 minutes (30°C)
Dry Hard36 hours (5°C)16 hours (20°C)10 hours (30°C)
Interval before OvercoatingMin.36 hours (5°C)16 hours (20°C)10 hours (30°C)
( by self )Max.10 days (5°C)7 days (20°C)5 days (30°C)
VOC Values321 g / L as supplied
ThinnerNIPPON MARINE THINNER 600 / NIPPON MARINE THINNER 615 (China Regions)

Application Method

Airless Spray

Tip range0.48 ~ 0.53 mm
Fan angle45 ~ 60°
( T/U )30° Output pressure 150 ~ 200 kg / cm²
BrushFor touching up small areas only
Mixing Ratio by VolumeBASE 3.57 / HARDENER 1
Pot Life after Mixing5 hours (5°C)
3 hours (20°C)21/2 hours (30°C)
PackagingTwo Packs Package may vary from country to country.
Japan Local BrandNIPPE EPOXY PC NOA
Flash PointBASE 34 °C, HARDENER 25 °C

Surface Preparation

Blast cleaned to ISO-Sa 21/2

is recommended.

Safety

Take precautions to avoid skin and eye contact (i.e. gloves, goggles, face masks, barrier creams etc.) Proper ventilation and protective measures must be provided during applications and drying period to keep solvent vapor concentrations within safe limits.

Prior to use, obtain, consult and follow the SDS for this product concerning health and safety information.

<Note>

1)The information contained in this sheet is liable to modification from time to time in the light of experience and our policy of continuous product development.

2)Apply this paint immediately after sandblasting. Before painting, the areas where corroded, welded and burnt should be carefully treated with sandblasting,shotblasting,or a disc sander or a power brush.

3)If half-dried painted surface is subjected to rain or dew, blooming or sweating may occur, with the surface turned to white. Rub the area lightly with a wire brush before painting.

4)For the applications, refer to our "Suitability Table of Cargoes for Loading" and "Application Manual of NOA PC System".

5) For availability of product consult Nippon Paint Marine representatives.

6) Unit size and filled volumes can vary due to local regulations.

7) Store the paints in paint store.

8) Use products that comply with local regulations to clean the paint equipment.

Data is subject to the manufacturer's latest version; in all cases the manufacturer's latest TDS prevails.

How many components does NOA PC have?
NOA PC is a two-component product. Mix it in the ratio given in the Coating Data table on this page before use.
What is the mixing ratio of NOA PC?
The mixing ratio of NOA PC is BASE 3.57 / HARDENER 1.
What dry film thickness is normally used for NOA PC?
The typical dry film thickness of NOA PC is 125-300 µm; the final value depends on the coating system and design requirements.
What is the theoretical spreading rate of NOA PC?
The theoretical spreading rate of NOA PC is 5.20 m²/L (125 µm); actual consumption depends on substrate roughness, application losses and colour hiding power.
What is the volume solids of NOA PC?
The volume solids of NOA PC is 65 ± 2%.
What is the VOC of NOA PC?
The VOC of NOA PC is 321 g / L as supplied.
Which thinner is used with NOA PC?
The recommended thinner for NOA PC is NIPPON MARINE THINNER 600 / NIPPON ….
Which standards does NOA PC relate to?
The technical data on this page states: ISO3233:1998 (see application instructions on this page). Specific applicability is subject to the manufacturer's technical data sheet and the recommended coating system.
Where can I buy NOA PC?
RichTech Industrial Technology (Shanghai) Co., Ltd. distributes industrial and marine coatings; NIPPON MARINE NIPPON MARINE is one of our regularly stocked brands, with coating selection, system design and quantity calculation support. Address: 10F, Changhui Building, 799 Yinxiang Road, Jiading District, Shanghai, China. Tel: +86 21 5056 8299 (9:00–21:00).