This product keeps the freshly active coating surface exposed to seawater, ensuring excellent antifouling performance under any sailing conditions. Parameters on this page: volume solids 59 ± 2%, theoretical spreading rate 5.90 m²/L.
Parameter source: nippon-marin original technical data sheet (TDS) 'FASTAR I'; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | — |
|---|---|
| Dry Film Thickness | — |
| Theoretical Spreading Rate | — |
| VOC | — |
| Density / Specific Gravity | — |
| Number of Components | One-component |
| Colour / Appearance | Overcoating interval (self) |
| Gloss | Maximum |
| Packaging Specifications | Safety |
The manufacturer's datasheet for this model does not state the coating position or resin type, so it has not been assigned to the above categories. Browse similar products by category, orContact Usconfirm the coating system.
| Publication date | August 2023 (ES) |
|---|---|
| FASTAR | FASTAR I uses its unique hydrophilic/hydrophobic nanostructure to control the precise, continuous and uniform release of biocide ions, achieving a stable and precise polishing effect. The acrylic silane polymer resin achieves long-term effective antifouling with low friction. |
This product keeps the freshly active coating surface exposed to seawater, ensuring excellent antifouling performance under any sailing conditions
| Suitable applications | Theoretical Spreading Rate |
|---|---|
| Ocean-going vessels | 5.90 m2/ L (100 µm) |
| Type | Drying Time |
| Nanostructure / special acrylic silane polymer (low friction) | Surface Dry |
| / high solids / hydrolysing / tin-free | 1 h (5 °C) 40 min (20 °C) 30 min (30 °C) |
3 h (5 °C) 1 h (20 °C) 40 min (30 °C)
| Colour | Overcoating interval (self) |
|---|---|
| Reddish brown, dark brown | Minimum 6 h (5 °C) 4 h (20 °C) 3 h (30 °C) |
| Gloss | Maximum |
| Semi-gloss | --- (5°C) --- (20°C) --- (30°C) |
| Volume Solids | Immersion interval (100 µm) |
| 59 ± 2% (ISO3233:1998) | Minimum 18 h (5 °C) 12 h (20 °C) 10 h (30 °C) |
| Dry Film Thickness | *Refer to precaution 4. |
| 80 ~ | 150 µm |
| Wet Film Thickness | NIPPON MARINE THINNER 300 |
|---|---|
| 136 ~ 254 µm | (0~5% by volume) 1/2 |
| Application Methods | Surface Preparation |
| Airless Spray | All surfaces to be coated must be clean, dry and free from contamination |
| Gun tip size | | 0.64 ~ 0.74 mm |
or peeling or other defects.
| Spray fan angle | | 45° ~ 54° |
|---|---|
| Output pressure | | 150 kg/cm² or above |
| Brush / roller | High-pressure fresh water washing to remove all grease, soluble salts, |
| For small-area repair only | rust or foreign matter |
| Packaging | Safety |
| One-component | Take precautions to avoid skin and eye contact (i.e. gloves, |
| Packaging may vary by place of production | goggles, face shields, barrier creams, etc.) |
| FASTAR I | During application and drying, adequate ventilation and protective measures must be provided to keep the solvent vapour concentration within safe limits. |
|---|
24 °C. Before use, obtain, consult and follow the health and safety information in the product's safety data sheet.
Precautions: 1. The content of this product data sheet may be revised at any time as our experience grows and the product is further developed.
| 2. Before and after spraying, clean with THINNER | 300 to clean the spray equipment, lines and guns. |
|---|
3. If this product is mixed with other antifouling paints or any other chemicals, the "tin-free declaration" for antifouling paint cannot be obtained.
4. The immersion interval is affected by environmental conditions, ventilation, film thickness and number of coats; consult field technical service for actual data. 5. The product should be stored in a paint warehouse.
2 / 2
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.