ECOLOFLEX SPC 200 Antifouling 200 is an antifouling paint. This product is a copper silyl acrylate polymer, hydrolysis-type tin-free self-polishing antifouling paint developed with proprietary technology; it enhances anti-algae performance and is suitable for conventional ocean-going vessels. Parameters on this page: volume solids 62 ± 2%, theoretical spreading rate 6.21 m²/L (100 µm DFT).
Parameter source: nippon-marin original technical data sheet (TDS) “ECOLOFLEX SPC 200 (Z) Antifouling 200”; spreading rate and other values are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 62 ± 2% |
|---|---|
| Dry Film Thickness | 65µm ~ 150µm |
| Theoretical Spreading Rate | 6.21 m²/L (100 µm DFT) |
| VOC | — |
| Density / Specific Gravity | — |
| Number of Components | — |
| Flash Point | 28°C |
| Thinner | THINNER 300 (thinning by weight: 0–5%) |
| Colour / Appearance | Brown Z — BPC006, light brown Z — BPB008 |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
This product is a copper silyl acrylate polymer, hydrolysis-type tin-free self-polishing antifouling paint developed with proprietary technology; it enhances anti-algae performance and is suitable for conventional ocean-going vessels. Extensive service records of the ECOLOFLEX SPC series demonstrate that this product delivers stable antifouling performance over the long term.
Antifouling paint for conventional ocean-going vessels
| Type | Cuprous oxide / copper silyl acrylate polymer (tin-free / self-polishing / hydrolysis-type / high solids) |
|---|---|
| Colour | Brown Z — BPC006, light brown Z — BPB008 |
| Gloss | Semi-gloss |
| Solids content (by volume) | 62 ± 2% (ISO3233:1998) |
| Recommended film thickness | DFT: 65–150 µm |
| Wet film | 105µm ~ 242µm |
| Theoretical Spreading Rate | 6.21 m²/L (100 µm DFT) |
| Thinner | THINNER 300 (thinning by weight: 0–5%) |
| 5°C | 20°C | 30°C | ||
| Drying Time | Surface Dry | 1 h | 40 min | 30 min |
| Hard Dry | 3 h | 1 h | 40 min | |
| Recoat interval | Minimum | 6 h | 4 h | 3 h |
| (self-recoat) | Maximum | ----- | ----- | |
| Interval before immersion (100 µm) | 18 h | 12 h | 10 h |
※Note 4)
| Flash Point | 28°C |
|---|
Airless spray: tip size 0.69–0.84 mm
| Spray fan angle | 62 ~ 75° |
|---|---|
| Output pressure | Above 150 kg/cm² |
| Brush/roller | For small-area repair only |
All surfaces to be coated must be clean, dry and free of contaminants. Wash with high-pressure fresh water to remove all oil, grease, soluble salts and foreign matter
| Packaging Specifications | 20 L |
|---|
Take the necessary protective measures to avoid skin and eye contact (e.g. gloves, safety glasses, face
1) The content of this product data sheet may be changed at any time as experience increases and product development continues. 2) When switching to other paints during application, clean spray equipment and lines with thinner (THINNER 300). 3) If this product is mixed with other antifouling paints or any other chemicals, the "tin-free certificate for antifouling paint" cannot be obtained. 4) The interval before immersion depends on ambient conditions, ventilation, film thickness and number of coats, and will be affected accordingly. Contact us for actual application.
5) Store this product in a paint warehouse
Data is subject to the manufacturer's latest version; in all cases the manufacturer's latest TDS prevails.