HEMPEL Water-borne Acrylic High-build Enamel 58030 is a water-borne coating used as a topcoat. In indoor and outdoor moderate to severe corrosive environments, it is used as a high-gloss topcoat in water-borne paint systems. After drying, it forms a non-yellowing high-gloss coating with low dirt pick-up, good weather resistance and high gloss retention. Parameters on this page: volume solids 40 ± 2%, dry film thickness 75 µm, theoretical spreading rate 5.3 m²/L. Comparable products of the same brand: HEMPEL Water-borne Acrylic Exterior Topcoat 380, HEMPEL Water-borne Epoxy-modified Interior Topcoat 320, HEMPEL Water-borne Polyurethane Topcoat 580.
Parameter source: HEMPEL original technical data sheet (TDS) "Hemucryl Enamel HI-Build 58030"; values such as spreading rate are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 40 ± 2% |
|---|---|
| Dry Film Thickness | 75 µm |
| Theoretical Spreading Rate | 5.3 m²/L |
| VOC | 51 g/L (China) |
| Density / Specific Gravity | 1.2 kg/L |
| Number of Components | — |
| Flash Point | 95°C |
| Colour / Appearance | White 10000 |
| Gloss |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
Hemucryl Enamel HI-Build 58030 is a water-borne acrylic dispersion coating. After drying it forms a non-yellowing high-gloss coating with low dirt pickup, good weather resistance and high gloss retention. It is particularly suitable for airless spray application.
Complies with EU Directive 2004/42/EC "on the limitation of emissions of volatile organic compounds due to the use of organic solvents in certain paints and varnishes and vehicle refinishing products: Subcategory i".
Used as a high-gloss topcoat in water-borne paint systems in indoor and outdoor environments of moderate to severe corrosivity. When used on buildings, the relatively high diffusion resistance to water vapour and carbon dioxide shall be considered. For handrails and similar parts, chemically curing coatings are recommended.
- When used as part of the specified coating system, it is approved as a low flame-spread material. For further details, see the Declaration of Conformity at hempel.com.
- Third-party verified, product-specific Environmental Product Declaration (Type III EPD, ISO 14025, EN 15804)
| Product safety | Flash point 95 °C |
|---|
| Regulations | Value |
| European Union | 51 g/L |
| USA (coatings) | 51 g/L |
| USA (regulatory) | 118 g/L |
| Canada | 51 g/L |
| China | 51 g/L |
| Hong Kong | 118 g/L |
| South Korea | 51 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. ªEU Directive 2004/42/CE. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 58030 |
|---|---|
| Standard colour* / code | White 10000 |
| Gloss | |
| Volume solids | 40 ± 2% |
| density | 1.2 kg/L |
| Recommended dry film thickness | 75 µm |
For further details, refer to the separate Hempel document Surface Preparation Guide.
Stir thoroughly before use.
Thinner
Fresh water
Hempel's Cleaner 98701
| Tools | Maximum thinning volume | Application parameters |
| Airless Spray | 0% | Nozzle pressure: 13 MPa Nozzle tip size: 0.38–0.48 mm |
| Brush | 0% | Not applicable. |
If brush or roller application is used, Hemucryl Brush Agent 99810 is required. If brush or roller application is used, multiple coats are required to achieve the specified dry film thickness. Spray parameters are indicative and may be adjusted according to site conditions. Pressure values apply to the material at 20 °C. (*Consult our representative if other application methods are required!).
| Specification range | Low | High | Recommended |
| Wet Film Thickness | 125 µm | 250 µm | 190 µm |
| Theoretical Spreading Rate | 7.9 m²/L | 4 m²/L | 5.3 m²/L |
Depending on the use and area of application, other film thicknesses than those indicated may be specified. This will change the spreading rate, drying and curing times and recoating intervals. Excessive thickness must be strictly controlled; locally, 140 µm [5.5 mils] DFT must never be exceeded. In cases of irregular surfaces, particular attention is recommended to avoid over-application.
- Previous coat: According to Hempel's specification. Recommended products: Hemucryl Enamel HI-Build 18302, Hempel's Water-borne Epoxy 18500 - Subsequent coat: None.
| Surface temperature | 20°C |
| Surface Dry | 18 min |
| Through dry | 60 min |
Measured at 75 µm dry film thickness under standard conditions; see Hempel's explanatory notes.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
| Ambient temperature | 25°C |
|---|---|
| Product | 12 months |
When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.
- The product must be stored in accordance with local legislation at a temperature not exceeding 35 °C [95 °F], protected from direct sunlight and from the direct influence of rain and snow.
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
| GWP (Global Warming Potential) | 8.2 g CO₂e/m² |
|---|
Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².
The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.
Calculated based on the standard colours defined in this PDS. Values may vary with colour.
For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:
This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.