Hempel Epoxy Zinc-rich Primer 174CN is a zinc-rich primer of the epoxy coating system. It can be used as a primer in epoxy, polyurethane and acrylic coating systems for steel surfaces in medium to severe corrosive environments. Hempel Epoxy Zinc-rich Primer 174CN is a two-component zinc-rich epoxy primer. Parameters on this page: volume solids 65 ± 2%, dry film thickness 50 µm, theoretical spreading rate 13 m²/L. Comparable products of the same brand: Hempel Epoxy Zinc-rich Primer, Hempel Zenit Epoxy Zinc-rich Primer 550, Hempel Zenit Epoxy Zinc-rich Primer 650.
Parameter source: HEMPEL original technical data sheet (TDS) "Hempel Epoxy Zinc-rich Primer 174CN"; values such as spreading rate are converted from TDS parameters for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 65 ± 2% |
|---|---|
| Dry Film Thickness | 50 µm |
| Theoretical Spreading Rate | 13 m²/L |
| VOC | 329 g/L (China) |
| Density / Specific Gravity | 2.5 kg/L |
| Number of Components | Two-component |
| Flash Point | 24°C |
| Thinner | HEMPEL's Thinner 08450 |
| Colour / Appearance | Grey-red 19830 * |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
174CN
Hempel Epoxy Zinc-rich Primer 174CN is a two-component zinc-rich epoxy primer. It forms a hard, abrasion-resistant and highly weather-resistant film. The product provides cathodic protection to locally damaged areas.
Can be used as a primer in epoxy, polyurethane and acrylic coating systems for steel surfaces in medium to severe corrosive environments.
| Product safety | Flash point 24 °C |
|---|
| Regulations | Value |
| European Union | 329 g/L |
| USA (coatings) | 329 g/L |
| USA (regulatory) | 329 g/L |
| China | 329 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 174CN |
|---|---|
| Product components | Base 174C9 |
Curing Agent 97040
| Standard colour / code | Grey-red 19830 * |
|---|
Grey 19830
| Gloss | Flat |
|---|---|
| Volume solids | 65 ± 2% |
| density | 2.5 kg/L |
| Recommended dry film thickness | 50 µm |
174CN
- The maximum permitted water-soluble salt level tested in accordance with ISO 8502-9 is 50 mg/m² (as NaCl).
- Use high-pressure fresh water washing (approx. 30 MPa [4400 psi]) combined with scrubbing to remove zinc salt deposits and white rust.
- Before final painting, all shop primer breakdown and contamination incurred during storage and erection must be thoroughly cleaned by mechanical/chemical means.
For further details, refer to the separate Hempel document Surface Preparation Guide.
Base 174C9 : Curing agent 97040 (4 : 1 by volume)
Products containing floating or settling particles/pigments require continuous stirring during application; this is especially important when heavily thinned.
| Thinner | HEMPEL's Thinner 08450 |
|---|---|
| Cleaning solvent | HEMPEL's Tool Cleaner 99610 |
| Product temperature | 20°C |
|---|---|
| Pot Life | 2 h |
| Tools | Application parameters |
|---|
Nozzle pressure: 15 MPa
Nozzle size: 0.43–0.53 mm
| Air Spray | Not applicable. |
|---|---|
| Brush | Not applicable. |
If brush or roller application is used, several coats may be required to achieve the specified dry film thickness. Keep thinning to a minimum. At low temperatures, additional thinning may be required, resulting in lower film build and slower drying. Spray parameters are indicative and may be adjusted to suit site conditions. Pressure figures apply to the material at 20 °C. (*For other application methods, consult the company representative.)
| Specification range | Low | High | Recommended |
| Wet Film Thickness | 61 µm | 123 µm | 77 µm |
| Theoretical Spreading Rate | 16 m²/L | 8.1 m²/L | 13 m²/L |
Depending on the application and area of use, other film thicknesses than those indicated may be specified. This will change the spreading rate, drying and curing times and recoating intervals. The actual consumption factor may vary with application conditions, equipment and skill. Excessive thickness must be strictly controlled; locally, 100 µm [4.0 mils] DFT must never be exceeded. In cases of irregular surfaces, particular attention is recommended to avoid excessive use.
174CN
- If brush or roller application is used, more coats are required to achieve the specified dry film thickness.
- Subsequent coat: in accordance with Hempel's specifications. Hempel's Epoxy MIO 471CN, Hempadur Mastic 45880
| Surface temperature | 20°C |
| Surface Dry | 30 min |
| Through dry | 90 min |
| Fully cured | 7 days |
Measured at 50 µm dry film thickness under standard conditions; see Hempel's explanatory notes. To determine the drying state, refer to the Application Specification COP FP1401-1 (drying test for high film thickness)
Hempel's specifications supersede all guidance shown in the recoat table.
| Product name | 10°C | 20°C | 30°C | 40°C | |
| Atmospheric, mild | |||||
|---|---|---|---|---|---|
| HEMPEL's Epoxy MIO 471CN | Minimum | 3 h | 90 min | 70 min | 45 min |
| Maximum | Extendable* | ||||
| Atmospheric, moderate | |||||
| HEMPEL's Epoxy MIO 471CN | Minimum | 4 h | 2 h | 90 min | 60 min |
| Maximum | Extendable* | ||||
Extendable* Depending on the actual exposure conditions, the coated surface may be recoated after an extended time. Contact your local Hempel representative for advice.
For products of the same generic chemical composition, recoat times are for reference only.
For further information, refer to Hempel's specifications.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
| Ambient temperature | 25°C |
| Binder | 12 months |
| Curing agent | 36 months |
When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.
- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
| GWP (Global Warming Potential) | 12.9 g CO₂e/m² |
|---|
Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².
The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.
174CN is calculated based on the standard colour codes defined in this PDS. Values may vary with different colour codes.
For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.