Interdur 8862 Acrylic Polysiloxane Topcoat is an acrylic paint, used as a topcoat. Suitable for newbuilding and maintenance projects in a variety of environments. A low-VOC, high-performance, two-component, isocyanate-free acrylic topcoat with excellent weather resistance and long-term overcoating performance. Although the low-molecular-weight reactive co-reactant becomes part of the film when cured under normal ambient conditions, analysis by EPA Method 24 has shown that it also affects the VOC value. Parameters on this page: volume solids 64% ± 2%, dry film thickness 50–75 µm (2–3 mils), theoretical spreading rate 12.80 m²/L.
Data source: AKZONOBEL original Technical Data Sheet (TDS), "Interdur 8862 Acrylic Polysiloxane Topcoat"; spreading rate and other values are converted from the TDS parameters, for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 64% ± 2% |
|---|---|
| Dry Film Thickness | 50–75 µm (2–3 mils) |
| Theoretical Spreading Rate | 12.80 m²/L |
| VOC | 2.67 lb/gal (320 g/L) US EPA Method 24 26… |
| Density / Specific Gravity | 1.25 kg/L (10.4 lb/gal) |
| Number of Components | Two-component |
| Thinner | Not recommended |
| Mixing Ratio | 7 parts : 1 part (by volume) |
| Gloss |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
A low-VOC, high-performance, two-component, isocyanate-free acrylic topcoat with excellent weather resistance and long-term overcoating performance.
Suitable for newbuilding and maintenance projects in a variety of environments.
8862
| Gloss | |
|---|---|
| Volume Solids | 64% ± 2% |
| Typical thickness | Dry film thickness 50–75 µm (2–3 mils), equivalent to wet film thickness 78–117 µm (3.1–4.7 mils) |
| Theoretical Spreading Rate | At 50 µm dry film thickness and the stated volume solids, 12.80 m²/L; at 2 mil dry film thickness and the stated volume solids, 513 sq ft/US gal |
| Practical Spreading Rate | Allowing for a suitable loss factor |
| Application Methods | Suitable for airless spray, air spray, brush, roller. Drying time; recommended topcoat recoat interval |
| Temperature | Surface Dry | Hard Dry | Minimum | Maximum |
| 10°C (50°F) | 3.5 h | 7 h² | 7 h | Unlimited¹ |
| 15°C (59°F) | 3 h | 7 h² | 7 h | Unlimited¹ |
| 25°C (77°F) | 2.5 h | 6 h² | 7 h | Unlimited¹ |
| 40°C (104°F) | 1 h | 3 h² | 3 h | Unlimited¹ |
¹ See the "Definitions and Abbreviations" section of International Paint's Protective Coatings division. ² Sufficient film strength has been achieved to allow handling and treatment of the coated steel structure.
Drying time is affected by relative humidity. The higher the relative humidity, the faster the drying. The quoted drying times were measured at the specified temperature and 50% relative humidity. The drying time data at 10 °C (50 °F) was measured at 80% relative humidity.
| Flash point (typical) | Component A 35 °C (95 °F); Component B 24 °C (75 °F); mixed 30 °C (86 °F) |
|---|---|
| Product weight | 1.25 kg/L (10.4 lb/gal) |
| Volatile Organic Compounds | 2.67 lb/gal (320 g/L) US EPA Method 24; 267 g/kg EU Solvent Emissions Directive content, Commission Directive 2010/75. Coating hazardous substances: GB 30981.2-S-Pb≤90-C compliant with GB 30981.2-2025. For more details, see the "Product Characteristics" section. |
All surfaces to be coated must be clean, dry and free of contaminants. Before application, all surfaces must be assessed and prepared in accordance with ISO 8504:2000.
Primed surfaces: Interdur 8862 should always be applied over a recommended anti-corrosive primer. The primer surface should be dry and free of contamination, and Interdur 8862 must be applied within the specified overcoating interval (see the relevant product data sheet).
Areas of spalling and damage etc. shall be treated to the specified standard (e.g. Sa 2½ (ISO 8501-1:2007) or SSPC-SP6 blast cleaning, or SSPC-SP11 manual/power tool cleaning), and these areas touched up with primer before applying Interdur 8862.
| Mixing | This product is supplied in two containers forming one unit. Mix the two components in the specified ratio in one operation. Once mixed, use within the specified pot life. |
|---|
(1) Stir the base (Component A) with a power mixer.
(2) Mix all of the curing agent (Component B) with the base (Component A) and stir thoroughly with a power mixer.
| Mixing ratio | 7 parts : 1 part (by volume) |
|---|
| Pot life | 10°C (50°F) | 15°C (59°F) | 25°C (77°F) | 40°C (104°F) |
| 4 h | 2 h | 1 h |
| Suitable for airless spray | Recommended nozzle diameter 0.35–0.45 mm (14–18 mils); total paint pressure at the nozzle not less than 155 kg/cm² (2204 lb/in²). |
|---|
| Air Spray | Recommended | Spray gun | DeVilbiss MBC or JGA |
| Air nozzle | 704 or 765 | ||
| (with pressure pot) | Spray painting | E | |
| Air spray (conventional) | Recommended | Use suitable dedicated equipment. | |
| Brush | Recommended | Typical thickness 40 µm (1.6 mil) | |
| Roller application | Recommended | Typical thickness 40 µm (1.6 mil) | |
| Thinner | Not recommended |
| Cleaner | International GTA007 |
|---|---|
| Interruption of work | Do not leave paint in hoses, spray guns or spray equipment. Flush all equipment thoroughly with International thinner. |
Once mixed, paint should not be resealed. If work is interrupted for too long, mix a fresh batch for application.
| Cleaning | All equipment should be cleaned immediately after use with International thinner. Flushing spray equipment periodically during daily work is good practice. Cleaning frequency depends on the volume sprayed, temperature, spraying time, including delays, and other factors. |
|---|
All surplus paint and empty containers must be disposed of in accordance with the relevant local laws/regulations.
The gloss level of the topcoat depends on the application method. Avoid mixed application methods. The optimum gloss and appearance are always obtained by conventional air spray.
Apply in good weather conditions. The surface to be coated must be at least 3 °C (5 °F) above the dew point; below 10 °C (50 °F), the product will not cure adequately.
When applying Interdur 8862 in confined spaces, ensure adequate ventilation.
Interdur 8862 reacts with atmospheric moisture, so the cans should be kept closed at all times. If the cans are left open, the paint will skin and lose its pot life. Partial mixing is not recommended.
Condensation on the surface during or after application will cause loss of gloss and a poor-quality film.
Premature exposure to standing water may cause colour change, especially for dark colours and at low temperatures.
Interdur 8862 is not suitable for immersion.
Thinning may adversely affect film appearance and performance; consult International Paint for further advice.
Note: VOC values are typical and for guidance only. They may vary with colour and general production tolerances.
Although the low-molecular-weight reactive additive becomes part of the film when cured under normal ambient conditions, analysis by EPA Method 24 shows that it also affects the VOC value.
The following primers are suitable for Interdur 8862:
| Intercure 200 | Intergard 251HS |
|---|---|
| Intercure 200HS | Intergard 475HS |
| Intercure 420 | Interplus 356 |
| Intergard 251 | Interzone 505 |
| Intergard 269 | Interzone 954GF. Interdur 8862 is normally overcoated with itself; for other suitable topcoats, consult International Paint. |
| For further information on the industry standards, terms and abbreviations used in this datasheet, see www.international-pc.com | In the following documents on the website: • Definitions and abbreviations • Surface preparation • Coating application • Theoretical and practical spreading rate. These sections are also available as separate publications on request. |
|---|
This product must be applied at the production site by professional applicators in accordance with the recommendations in this manual, the Material Safety Data Sheet and the instructions on the container label. Do not use this product without first reviewing the Material Safety Data Sheet (MSDS) that International Paint provides for its customers.
All work related to the application and use of this product must be carried out in accordance with the relevant national health, safety and environmental standards and regulations.
If welding or flame cutting is required on metal coated with this product, dust and fumes will be generated; use appropriate personal protective equipment and adequate local ventilation.
If in doubt about the suitability of this product for the intended use, consult AkzoNobel for further advice.
| Packaging Specifications | Component A | Component B | ||
| Volume | Packaging | Volume | Packaging | |
| 20 L | 17.5 L | 20 L | 2.5 L | 5 L |
For other packaging sizes, contact AkzoNobel.
| Packaging Specifications | Component A | Component B |
| 20 L | 24.57 kg | 2.66 kg |
| Shelf life | 12 months at 25 °C (77 °F). Thereafter, inspection is required. Store in a dry, cool environment away from heat and sources of ignition. |
|---|
© 2026/5/26 AkzoNobel. All rights reserved.
All registered trademarks mentioned in this publication are licensed to or owned by AkzoNobel.
www.international-pc.com
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.